Анотація

In aqueous solutions, a nanostructured AgAu bimetallic system is deposited by galvanic replacement on silicon. It was established that the coprecipitation of metals during galvanic replacement occurs somewhat ahead of the gold content in the AgAu/Si system. Thus, in aqueous solutions of [2mМАgNO3]:[10mМHAuCl4], nanoparticles with a ratio of Ag:Au = 2:10 are deposited on the silicon surface, respectively. The size of discrete bimetallic nanoparticles increases with increasing [AgNO3]:[HAuCl4] ratio. Therefore, at a close metal content, AgAu particles are the smallest. This is due to the factor of mutual influence of two metals during coprecipitation.

Ключові слова (англійською)
Автор (співавтори)
Ім'я Прізвище Приналежність до організації E-mail Номер телефону ORCID ID Вчене звання, посада Адреса організації Внесок автора(ів) Приналежність до організації
Mariana
Shepida
mariana.v.shepida@lpnu.ua
0000-0001-9842-5864
Lviv, S. Bandera Street 12
Написання – оригінальний рукопис
Lviv Polytechnic National University
Vitalii
Tsybrivskyi
vitalii.tsybrivskyi.hb.2023@lpnu.ua
Lviv, S. Bandera Street 12
Дослідження
Lviv Polytechnic National University
Yurii
Sukhatskyi
yurii.v.sukhatskyi@lpnu.ua
Lviv, S. Bandera Street 12
Формальний аналіз
Lviv Polytechnic National University
Martyn
Sozanskyi
martyn.a.sozanskyi@lpnu.ua
Lviv, S. Bandera Street 12
Методологія
Lviv Polytechnic National University
Vasyl
Kordan
vasyl.kordan@lnu.edu.ua
Lviv, 6, Kyryla i Mefodiya St.,
Візуалізація
Ivan Franko National University of Lviv
Файл рукопису
si.doc1.45 МБ