Chemical Ni–Co–P Deposition and Low-Temperature Heat Treatment of Joint Parts for Hand Rehabilitation Exoskeletons

Abstract

This paper considers surface strengthening of kinematic-pair parts of hand rehabilitation exoskeletons within the functionally oriented technological process framework of Applied Mechanics (G9). Chemical (electroless) deposition of a Ni–Co–P coating is proposed in two variants: as-deposited, and with subsequent heat treatment at 400 °C for 1 h, which precipitates the Ni3P phase and raises coating microhardness. Process temperatures do not exceed 400 °C, so slender parts keep their dimensions without distortion. Criteria for assigning each variant to exoskeleton elements and a process route for joint pins are formulated.

Author (co-authors)
First name Last name Institutional affiliation E-mail Phone number ORCID ID Academic status, position Institution address Author contribution(s) Institutional affiliation
Volodymyr
SHEVCHUK
vov4ik.bratik@gmail.com
PhD Student
12 S. Bandery Street, Lviv, 79013, Ukraine
Conceptualization
Investigation
Writing – Original Draft Preparation
Lviv Polytechnic National University
Andrew
Stetsko
andrii.y.stetsko@lpnu.ua
0000-0002-6772-1860
Associate Professor
12 S. Bandery Street, Lviv, 79013, Ukraine
Methodology
Supervision
Writing – Review & Editing
Lviv Polytechnic National University